PRODUCTION PROCESSES FOR CRGO TOROIDAL TRANSFORMER CORES
|
|
|
|
SLITTING :
CRGO
Electrical steel comes in the form of wide coils having widths
of 750 mm to 1000 mm. These coils are to be slit in various
widths in steps ranging from 10 mm to 100 mm.
|
|
WINDING :
These slit coils of CRGO are wound on semi automatic winding machine as per the dimensions given
by our customers.
|
|
SPOT WELDING :
On winding the CRGO Toroidal cores to the exact size the start and finished ends of the core are
spot welded on spot welding machine.
|
|
STRESS RELIEF ANNEALING :
During the winding process of CRGO, severe stresses are induced in the gains of the raw material. Theses stresses are relieved in our specially designed annealing furnace equipped
with automatic temperature controller, circulating fan and inert atmosphere. The annealing cycle (at 800°C)
improperly controlled to get uniform and best annealing results.
|
|
TESTING :
Since the CRGO electrical properties of cores are very critical, every core is tested on a specially designed test bench. The ampere turns/cm (magnetization current) are measured on every core to
ensure that they are within the specified limits.
|
|
PAINTING :
After testing the 'PASSED' cores are painted with N.C. paint to prevent the
CRGO Toroidal cores from corrosion.
|
|
PACKING :
The Electrical Properties of CRGO Toroidal cores are very sensitive to bad handling during transit. We take great care while packing the cores in wooden boxes with cushioning material to prevent stresses on the cores during dispatch.
|
|
|
|
|
SLITTING :
The Slitting Machine gives 18 adjustable strip widths. Tool geometry is of critical importance for eliminating burrs
of CRGO.
|
|
CUTTING ACCORDING TO LENGTH (CRGO) :
|
|
AUTOMATIC METHOD OF PROCESSING CRGO POWER
TRANSFORMER CORES : |
Nomax Electrical Steel Pvt. ltd. uses the newest, computerized version of
Cut to Length Machines in order to produce Step Lap
Transformer Laminations Cores. |
|
MANUAL METHOD USED FOR DISTRUBUTION CRGO
TRANSFORMER CORES : |
The SECOND stage of the manufacturing process is "Shearing" at 45 or 90 as required by the customer. Strict tolerances are maintained (as per the
tolerance chart) and a unique three point location method ensures accuracy in dimensions in terms of angle and length. Burs are controlled by ensuring the blades are always sharp. Continuous line inspection ensures all parameters are strictly maintained within acceptable limits.
|
|
The THIRD step of the manufacturing process is to fabricate "V-Notch" or holes at per customer's
design. Accuracy is utmost importance and specially designed jigs and fixtures ensure that all dimensional tolerances specified by the customer are maintained.
|
|
STRESS RELIEF ANNEALING :
The FOURTH step of the manufacturing process of CRGO
Transformer Cores is to deburr and stress relief anneal the
material by other health annealing finance. This is done as
per the mill's specification at 820 º C for a few minutes
depending upon the thickness and grade of CRGO material.
|
|
TESTING :
Since the electrical properties of CRGO cores are very
critical, every core is tested on a specially designed test
bench. The ampere turns/cm (magnetization current) are
measured on every core to ensure that they are within the
specified limits.
|
|
PACKING :
We are able to deliver CRGO lamination as leg or sheet packet,
according to your packing requirements, inside of wooden box
or on the pallets.
|
|